EN36C
Grade Introduction:
EN36C Alloy Steel is a Nickel-Chromium Case hardening steel which is suitable for deep hardening to develop a touch core is suitable for gears, cams rollers available in diameters only. EN36C Alloy Steel is a carburizing steel grade with very high surface strength with a soft but strong core. The material retains a remarkable degree of toughness. With high tensile strength, EN36C is used in the production of numerous high-strength parts including crankshafts in the automotive and aerospace sector. En36C is used specifically in heavy-duty and highly stressed applications due to its hardenability toughness and high core strength. EN36C also offers excellent fatigue resistance. EN36C gives a hard case with a strong core, whilst retaining a remarkable degree of toughness.
Grade Application
As a carburizing steel grade, it is suitable for roller and ball bearings of an extra light section, airplane and motor crankshafts requiring hard surfaces for roller paths, connecting rods with case-hardened ends, as well as highly stressed gudgeon pins, gears, and certain types of collects.
Equivalent Grades
BS 970 1991 |
BS 970 1955 EN |
AISI/SAE |
WERKSOFF |
655M13 |
EN36 |
3415 |
1.5752 |
Addition to other grades
MS, EN1A, EN3B, EN8, EN8D, EN9, EN19, EN24, EN31, EN32B, EN36C, EN41B, EN43B, EN47, EN353, IS2062, 42Crmo4, HCHCR, D2, D3, H-11, H-13, CW-1, OHNS, M2, M35, M42, DIN1.2714, P20, P20+S, P20+Ni, SCM420, ASTMSA-36, ASTMSA-105, SAE1018, SAE4140, SAE8620, 16MNCR5, 20MNCR5, C20, C45, C50, C60, CK45, 20C8, 40C8, 45C8, 55C8, C55MN75, SAE52100, S40C, S355J2G3.
Our Supply Range
We supply to automotive ancillaries and OEM customers. The products we manufacture are used as input for manufacturing of automotive and general engineering components. These components are further assembled into systems fitted in automobiles and other engineering applications.
Product Type | Size Range |
---|---|
Forged Round Bars | 140mm Dia to 850mm |
Rolled Round Bars | 16mm Dia and above |
Forged Flat Bars | Thickness: 32mm to 510mm, Width: 65mm to 1050mm |
Rolled Flat Bars | Thickness: 6mm to 110mm, Width: 25mm to 510mm |
Chemical Composition
The following table shows the chemical composition of EN36C steel:
Element |
C |
Mn |
Si |
Ni |
Mo |
Cr |
S |
P |
Content (%) |
0.12-0.18 |
0.30-0.60 |
0.10-0.35 |
3.00-3.75 |
0.10-0.25 |
0.60-1.10 |
0.05 Max |
0.05 Max |
Heat Treatment
Heat treatment temperatures, including the rate of heating, cooling, and soaking times will vary due to factors such as the shape and size of each EN36C steel component. Other considerations during the heat treatment process include the type of furnace, quenching medium, and workpiece transfer facilities. Please consult your heat treatment provider for full guidance on heat treatment of EN36C case hardening steel.
Hardness
341
Hardening
En19 alloy steel can be hardened by cold working or heating and quenching.
Forging Properties
Soak for 1 hour at 2150 F (1177 C) prior to forging. Do not work below 1850 F (1010 C). Post-work solution treatment is required prior to final hardening.
Stress Relieving
Heat to 600°C – 650°C, Cool in still air.
Welding
Readily weldable in the annealed supplied condition.
Machinability
En36C offers very good machinability and weldability when supplied in the annealed condition, although when welded the material should be stress relieved after cooling. Welding is not however recommended in the heat-treated or carburized condition. Machinability options including turning, milling, drilling, and tapping are all suitable as long as the tool type, feeds and speeds are used in accordance with the machine manufacturer’s recommendations.
Mechanical Properties
Tensile StrengthN/ mm² |
Elongation % |
Impact Izod J |
ImpactKCV J |
HardnessHB |
Reduction of Area % |
1100 |
15 |
40 |
35 |
341 |
50 |
Physical Properties
DENSITY (G/CM 3) |
8.08 |
DENSITY (LB/IN 3) |
0.292 |
MELTING POINT (°C) |
1425 |
MELTING POINT (°F) |
2600 |
Tempering
Temper in oil at a temperature of 150/200°C will alleviate stresses and the risks of cracking.
Thermal Properties
Temp. (°C) |
Modulus of elasticity (GPA) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) |
Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
13 |
– |
– |
0.23 |
– |
|||
697 |
912 |
– |
32.3 |
333 |
– |
||
634 |
– |
44 |
21.2 |
141 |
213 |
Normalizing
Heat to 890°C – 920°C, Cool in still air.
Annealing
Heat to 830°C – 850°C, Cool in a furnace.
Density
DENSITY (G/CM 3) – 8.08
Supply Cities
Ambattur, Bangalore, Chennai, Coimbatore, Dindigul, Guindy, Madurai, Nellore, Hyderabad, Tirupur, Tuticorin, Madurai, Andhra Pradesh, Karnataka, Puducherry, Kerala, Kanyakumari, Telangana, Salem, Thanjavur, Trichy, Erode, Vellore, Karur, Nagercoil, Kanchipuram, Karaikudi, Pudukottai, Nagapattinam.
People also search as
EN36C Steel Round Bar, EN36C Steel Round Bar Manufacturers, EN36C Steel Suppliers, EN36C Stockist, EN36C Steel Dealers, EN36C Steel Distributors, EN36C Wholesalers, EN36C Steel Traders, EN36C Steel Square Distributors, EN36C Steel Flat Bar, EN36C Steel Companies Near me.
EN36C, EN36C Steel, EN36C Chemical composition, EN36C Mechanical properties, EN36C Equivalent Grades, EN36C Steel plate, EN36C Steel sheet, EN36C Manufacturers, EN36C Suppliers, EN36C Dealers, EN36C Stockist, EN36C Distributors, EN36C Wholesalers, EN36C Traders.